EDM Type Comparison

ParameterDie Sinking (Rough)Die Sinking (Finish)Wire EDM
Current (A)10-600.5-51-4
On Time (us)100-5005-500.1-5
Off Time (us)30-10010-305-20
Surface FinishRa 6-15Ra 0.2-0.8Ra 0.1-0.4

Electrode

Graphite: rough machining, lower wear. Copper: fine finish, better surface. Copper-Tungsten: small details, high wear resistance.