Guide / Forging Types

Forging Types: Hot vs Cold

Shaping metal by compressive force for superior strength

Forging Temperature Comparison

TypeTemp (Steel)ToleranceStrength vs Machined
Hot Forging900-1250C+-1mm+15-25%
Warm Forging600-900C+-0.3mm+20-30%
Cold ForgingRoom temp+-0.05mm+30-50%

Design Rules

Draft angles: 3-7 deg (hot), 0-3 deg (cold). Min radius: 3mm hot, 1mm cold. Max section change: 3:1 per step.